facebook icon instagram icon linkedin icon

Our Products

PITSA owns and operates fuel receiving, storage and distribution facilities.

PITSA provide high quality Gasoline RON 92, with specification below:

No Parameter Units Limits Grade Test Method
Min Max
1 Sulphur mg/kg   150 All Grades ASTM D 0543
2 Research Octane Number (RON) --- 92   All Grades ASTM D 2699
3 Motor Octane Number (MON) --- 78   All Grades ASTM D 2700
4 Distillation, Final Boiling Point °C   210 All Grades ASTM D 86
5 Olefins % v/v   18 All Grades ASTM D 1319
6 Aromatic % v/v   42 All Grades ASTM D 1319
7 Benzene % v/v   3.0 All Grades ASTM D 5580
8 Lead mg/L   5.0 All Grades ASTM D 3237
9 Oxigen % m/m   2.7 All Grades (No Ethanol) ASTM D 4815
  3.5 All Grades (No Ethanol) ASTM D 4815
10 Ethanol % v/v   10 All Grades ASTM D 4815
11

Oxygenates Except Ethanol,

MTBE (Methyl Tertiary Butyl Ether)

ETBE (Ethyl Tertiary Butyl Ether)

TAME (Tertiary Amyl Methyl Ether)

DIPE (Diisopropyl Ether)

TAEE (Tert-Amyl Ethyl Ether)

Methanol

TBA (Tertiary butyl alcohol)

IBA (Iso-butyl alcohol)

%v/v   1.0 All Grades ASTM D 4815
12 Phosporus mg/L   1.3 All Grades ASTM D 3231
13 Copper Corrosion (3hrs at 50°C) Rating   Class 1 All Grades ASTM D 130
14 Existent Gum (Washed) mg/100ml   5.0 All Grades ASTM D 381
15 Induction Period minutes 360   All Grades ASTM D 525
16 Rapid Vapor Pressure kPa 45 65 All Grades ASTM D 323
17 Flexible Volatility Index index   100 All Grades ASTM D86 & ASTM D323

Ref: Timor Leste Regulation No 1/2004

No Parameter Units Limits Test Method
Min Max
1 Sulphur Content mg/kg   500 ASTM D5453
2 Catane Index --- 45.0   ASTM D4737
3

Density at 15°C

kg/mg3 820 850 ASTM D4052
ASTM D1298
4 Distilation T95 °C   360 ASTM D86
5 Polyaromatic Hydrocarbon (PAHs) % m/m   11 IP391
6 Ash Content % m/m   0.01 ASTM D482
7 Viscosity mm2/s 2.0 4.5 ASTM D445
8 Carbon residue (10% distilation residue) %m/m   0.2 ASTM D4530
9 Water Content mg/kg   200 ASTM D6304
10 Total Contamination mg/kg   24 EN 12662
11 Conductifity at Ambient Temperature pS/m 50.0 1.0 ASTM D2624
12 Oxidation Stability mg/L   25 ASTM D2274
13 Colour Rating   2.0 ASTM D1500
14 Copper Strip Corrosion (3 Hours at 50°C) Rating   Class 1 ASTM D130
15 Flash Point °C 61.5   ASTM D93
16 Filter Blocking Tendency Rating   2.0 ASTM D93
17 Fatty Acid Methyl Ester (FAME) %v/v   5.0 EN 14078
18 Lubricity mm   0.46 IP 450
No Parameter Units Limits Test Method
Min Max
1 Colour --- Report ASTM D 6045
2 Distilation ---     ASTM D 86
2.1 IBP °C Report
2.2 10% °C   205
2.3 20% °C Report
2.4 50% °C Report
2.5 End Point °C   300
2.6 Residue %vol   1.5
2.7 % Loss %vol   1.5
3 Flash point °C 38   IP 170
4 Density 15°C kg/l 0.7750 0.8400 ASTM D 1298
5 Freezing Point °C   Mminus 47 ASTM D 2386
6 Corrosin Copper Strip 2H/100°C class   1 ASTM D 130
7 Existent Gum mg/100 ml   7

ASTM D 381

8 Electrical Conductivity pS/m 50 600 ASTM D 2624
9 Microsearatometer, at point of Manufacturing       ASTM D 3948
9.1 MSEP without SDA Rating 85  
9.2 MSEP with SDA Rating 70  
No Parameter Units Limits Test Method
Min Max
1 Specific Gravity at 60/60°F --- Report ASTM D 1657
2 Vapor Pressure at 100°F psig   145 ASTM D 1267
3 Wathering Test at 36°F %vol 95   ASTM D 1837
4 Copper Corrosion 1 hr/100°F ---   ASTM No 1 ASTM D 1838
5 Sulphur Content grams/100 cuft   15 ASTM D 2784
6 Water Content --- No Free Water     Visual
7 Composition ---    

ASTM D 2163

7.1 C2 %vol   0.8
7.2 C3&C4 %vol 97  
7.3 C5+ %vol   2.0
8 Etil atau Butil Markaptan ml / 1000 AG 50   ASTM D-36
No Parameter Units Limits Test Method
Min Max
1 Specific Gravity at 60/60°F --- 1   ASTM D-70
2 Ductility at 25°C cm 100   ASTM D-133
3 Flash Point C.O.C °C 200   ASTM D-92
4 Loss on Heating at 5 Hours/163°C %wt   0.4 ASTM D-6
5 Penetration at 25°C 0.1mm 60 70 ASTM D-5
6 Penetration after Loss on Heating % 75   ASTM D-5
7 Solubility in CCL %wt 99   ASTM D-2042
8 Softening Point Ring and Ball °C 48 58 ASTM D-36